High-capacity automatic cutting machine Cutlam 4.0

  • Description
  • Specification
  • Consumables

Description

CUTLAM®4.0

The CUTLAM®4.0 is designed especially for manufacturing companies with high standards who are looking for high- quality and reliable equipment for heavy-duty use with a great cutting capacity.
La CUTLAM®4.0 is a pedestal-mounted single-block machine with an integrated recirculation/decanter tank. The wheel’s vertical descent can be controlled automatically (oleo pneumatic) or manually using the joystick. The maximum cutting descent is 240 mm.
Adapted for intensive use on heavy components, the CUTLAM®4.0 is fitted with a powerful 5.5 kW motor. The wheel’s speed is adjustable from 1000 to 4000 rpm, the feed speed is adjustable. 2 cutting modes are available: sequential automatic with adjustable frequency or continuous.
An end of cycle sensor shuts off the machine and automatically raises the wheel after each operation. The controls are easy to use and intuitive: they are centralized on the 5.7’’ arm-mounted touch-screen. The wide cast-iron clamp bench has 6 T-longitudinal grooves and 5 transversal grooves, and as an optional extra may be made mobile along the X and the A axes

Specification

WheelØ 300 to 400 mm
ShaftØ25,4mm
Standard flangesØ110 mm
Max cutting capacityØ 154 mm or 145 x 160 mm or 90 x 275 mm (with a Ø 400 mm wheel) + right and left opening for long parts)
Passage under the wheel190 mm (with a Ø 400 mm wheel)
Vertical movementManual

 

LubrificationRecirculation system, 140 litres, on casters

Cleaning system integrated, with a shower head outside of the cutting chamber

Motor power5,5 kW
Rotational speedVariable, from 1000 to 4000 rpm
Arm speed advance5 to 200 mm/min during cutting
TableDouble grooved treated cast iron, 400 x 400 mm
Type of grooveT groove 12 mm (6 longitudinal, 5 transversal)
LighteningLED
ProtectionCover with locking system
BodySteel coated with epoxy paint
Voltage400 Volts – 50 Hz (three-phase)
Dimensions (W x H x D)818 (+ 300 mm with control panel) x 1802 x 1280 mm
Weight650 kg
Reference60 CT40A 00