MASTERLAM 3.0 Automatic polishing machine with central and individual pressure

  • Description
  • Specification
  • Accessories
  • Consumables

Description

Automatic, single plate Ø 250 to 300 mm polishing machine, bidirectional rotation and variable speed.

This machine has all the functions that make the MASTERLAM® range outstand and on this model a specific new combo-head.

The MASTERLAM®3.0 is the metallographic polishing machine without concession. Polishing can be carried out with central pressure or individual pressure and can be equipped with a stock removal measuring system.

The MASTERLAM®3.0 is based on the same technology as the MASTERLAM®1.0 with, in this configuration, a powerful central and individual pressure head equipped with 6 pistons. Changing sample holders is quick and the pressure mode is controlled directly on the screen without having to touch the head, thus, you can switch from one pressure mode to another in a few seconds.

Specification

Plate capacity
Ø 250 to 300 mm
Body
Steel coated with epoxy paint
Bowl
Removable resin bowl for easy cleaning
Controls
Touch screen (5,7“)
Plate rotation speed
Variable from 20 to 650 rpm
Bidirectional rotation
Head’s speed
Variable from 10 to 150 rpm
Bidirectional rotation
Applicable load
5 to 400 N central pressure
5 to 100 N individual pressure
Capacity
Sample size 6 X Ø 40 mm
Sample size 1 – 6 X Ø 50 mm
Workspace lightening
LED
Water inlet
Removable pipe, with flow rate adjustment and safety solenoid valve
Programming
60 storable programs, USB connector to backup programs and Ethernet port for networking
Cumulative machine power
1.1 kW
Voltage
230 V – 50 Hz single phase
Pneumatic feed
6 bars
Dim. W x H x D
550 x 670 x 580 mm
Weight
85 kg

 

Accessories

Dosing unit DISTRILAM